TRANSITION OF THE LUBRICATED WEAR OF CARBON STEELIWAI Y; ENDO K.1982; WEAR; CHE; DA. 1982-01-01; VOL. 75; NO 1; PP. 159-172; BIBL. 12 REF.Conference Paper
ON THE SLIDING WEAR CHARACTERISTICS OF BORIDED STEEL SURFACESHIBUYA Y; IMAZAWA Y; KUWANA K et al.1979; TETSU TO HAGANE; JPN; DA. 1979-12; VOL. 65; NO 14; PP. 2057-2066; BIBL. 15 REF.Article
THE INFLUENCE OF HARDNESS DIFFERENCE ON THE FRICTIONAL AND WEAR BEHAVIOUR OF STEEL/COPPER ALLOY PAIRS IN PLANE SLIDING FRICTION UNDER MIXED FRICTION CONDITIONSKRAUSE H; TACKENBERG W.1980; WEAR; CHE; DA. 1980-11; VOL. 64; NO 2; PP. 291-302; BIBL. 5 REF.Article
POSSIBILITIES AND LIMITATIONS FOR THE APPLICATION OF CVD-COATED CEMENTED CARBIDE TOOLS AND STEEL TOOLS = EINSATZMOEGLICHKEITEN UND -GRENZEN FUER CHEMISCHE DAMPFBESCHICHTETE HARTMETALL- UND STAHLWERKZEUGE = POSSIBILITES ET LIMITES D'EMPLOI DES OUTILS EN ACIER ET CARBURE REVETUS PAR LE PROCEDE CHIMIQUE EN PHASE VAPEURSCHINTLMEISTER W; KANZ J; WALLGRAM W et al.1983; INT. J. REFRACT. HARD MET.; GBR; DA. 1983-03; VOL. 2; NO 1; PP. 41-43; BIBL. 7 REF.Conference Paper
EFFECT OF SPECIMEN THICKNESS ON THE CRACK PROPAGATION AND CRACK BRANCHING IN DELAYED FAILURENAKASA K; TAKEI H.1982; ENG. FRACT. MECH.; GBR; DA. 1982-03; VOL. 16; NO 3; PP. 387-392; BIBL. 9 REF.Article
REACTION BETWEEN S35C AND LIQUID ZINCKOGA H; UCHIYAMA Y; TSUCHIDA K et al.1982; TETSU TO HAGANE; JPN; DA. 1982-01; VOL. 68; NO 1; PP. 113-119; BIBL. 18 REF.Article
PROTEZIONE DELLE FORME METALLICHE PER LA PRESSOCOLATA = ABRASION PROTECTION OF PRESSURE DIE CASTING DIES1981; FONDERIA; ITA; DA. 1981-03; VOL. 30; NO 3; PP. 65Article
VERFAHREN ZUR PRUEFUNG VON STAHL AUF KORROSIONSDAUERFESTIGKEITPETROV LN; STEPURENKO YU V.1981; ZAVOD. (LAB); SUN; DA. 1981-10; VOL. 47; NO 10; PP. 72-73Article
WEAR AND FRICTION IN STEEL, ALUMINUM AND MAGNESIUM ALLOYS:PT. 1. PEARLITIC AND SPHEROIDIZED STEELSBHATTACHARYYA S.1980; WEAR; CHE; DA. 1980-06-02; VOL. 61; NO 1; PP. 133-141; BIBL. 8 REF.Article
AUTORADIOGRAPHIC STUDY ON BORONIZED STEEL = AUTORADIOGRAPHISCHE UNTERSUCHUNG AN BORIERTEM STAHL = ETUDE AUTORADIOGRAPHIQUE DE L'ACIER BRORUREBOZKURT N; GECKINLI AE; GECKINLI M et al.1983; MATER. SCI. ENG.; ISSN 0025-5416; CHE; DA. 1983-02; VOL. 57; NO 2; PP. 181-185; BIBL. 8 REF.Article
SCHLICHT-FORM- UND WAELZFRAESEN VON GROSSZAHNRAEDERN = FINISH FORM MILLING AND HOBBING OF LARGE GEAR WHEELSMENTE HP.1981; WERKSTATT BETR.; DEU; DA. 1981-06; VOL. 114; NO 6; PP. 379-383; BIBL. 2 REF.Article
UNTERSUCHUNGEN ZUM EINFLUSS MINERALISCHER ZWISCHENSTOFFE AUF DAS VERSCHLEISSVERHALTEN METALLISCHER GLEITPAARUNGEN = STUDIES ON THE INFLUENCE OF INTERMEDIATE MINERAL MATERIALS ON THE WEAR BEHAVIOUR OF METALLIC SLIDING COMBINATIONSGUENTER H; BESSER D.1981; FREIBERG. FORSCHUNGSH., REIHE B; DDR; DA. 1981; VOL. 222; PP. 63-73; BIBL. 8 REF.Conference Paper
HARD CHROMIUM DEPOSITION:PLATING LOW CURRENT DENSITY AREASGHOUSE M.1980; MET. FINISH.; USA; DA. 1980-01; VOL. 78; NO 1; PP. 55-58; BIBL. 4 REF.Article
OBSERVATION OF THE SLIDING WEAR TRACE OF BORIDED STEELSHIBUYA Y; IMAZAWA Y; KUWANA K et al.1980; TETSU TO HAGANE; JPN; DA. 1980-04; VOL. 66; NO 5; PP. 532-538; BIBL. 2 REF.Article
WEAR OF AISI 4340 STEEL UNDER BOUNDARY LUBRICATIONJAHANMIR S.1981; WEAR; CHE; DA. 1981-12-08; VOL. 74; NO 1; PP. 51-65; BIBL. 13 REF.Conference Paper
AN EVALUATION OF THRESHOLD STRESS-INTENSITY FACTOR, KISCC USING AE TECHNIQUENOZUE A; KISHI T; HORIUCHI R et al.1981; TETSU TO HAGANE; JPN; DA. 1981-08; VOL. 67; NO 10; PP. 1787-1794; BIBL. 31 REF.Article
THE FRETTING WEAR OF 0.45% STEEL AND AUSTENITIC STAINLESS STEEL FROM 20 TO 6500C IN AIRKAYABA T; IWABUCHI A.1981; WEAR; CHE; DA. 1981-12-22; VOL. 74; NO 2; PP. 229-245; BIBL. 25 REF.Conference Paper
EFFECTS OF TEMPERATURE, INITIAL STRESS INTENSITY FACTOR AND LOADING SPEED ON THE CRACK BRANCHING IN DELAYED FAILURENAKASA K; TAKEI H; YOSHIDA M et al.1980; ENG. FRACT. MECH.; GBR; DA. 1980-09; VOL. 13; NO 3; PP. 667-675, 677; BIBL. 23 REF.Article
FACTORS AFFECTING SCALE ADHESION ON STEEL FORGINGSZITTERMAN JA; BACCO RP; BOGGS WE et al.1982; J. MET.; USA; DA. 1982-04; VOL. 34; NO 4; PP. 22-26; BIBL. 9 REF.Article
ON THE STRESS CORROSION CRACK GROWTH RATES OF AISI 4340 STEEL NEAR ITS LOWER TEMPER MARTENSITE EMBRITTLEMENT RANGE IN 0.5 N NACL SOLUTION = UEBER DIE SPANNUNGSKORROSION-RISSWACHSTUMSGESCHWINDIGKEITEN VON STAHL AISI 4340 NAHE DES UNTEREN ANLASSMARTENSIT-VERSPROEDUNGSBEREICHES IN 0,5 N NACL-LOESUNG = SUR LA VITESSE DE CROISSANCE DE CRIQUES DE CORROSION SOUS CONTRAINTE DE LACIER AISI 4340 PRES DE LA REGION INFERIEURE DE FRAGILITE MARTENSITIQUE DE REVENU EN SOLUTION DE NACL 0,5 NTEWARI VK; WINAND R; CHARLIER J et al.1982; ARCH. EISENHUETTENWES.; DEU; DA. 1982-08; VOL. 53; NO 8; PP. 329-333; BIBL. 13 REF.Article
WATER VAPOR CONTRIBUTION TO THE EROSION OF STEEL BY HIGH TEMPERATURE FLOWSGANY A; CAVENY LH; JOHNSON JW et al.1981; TRANS. ASME, J. HEAT TRANSF.; USA; DA. 1981-05; VOL. 103; NO 2; PP. 383-386; BIBL. 6 REF.Article
ACCURACY IN END MILLINGTORII N; MATSUO K.1981; KOBE STEEL ENG. REP., RES. DEV.; JPN; DA. 1981-07; VOL. 31; NO 3; PP. 34-37; BIBL. 3 REF.Article
AN EVALUATION OF THE CHEVRON V-NOTCHED BEND BAR FRACTURE TOUGHNESS SPECIMENSHIH TT.1981; ENG. FRACT. MECH.; GBR; DA. 1981; VOL. 14; NO 4; 821-829, 831-832; BIBL. 16 REF.Article
REPETITIORIUM: SPANENDE FORMUNG = SURVEY COURSE: MACHININGFREY SR.1981; SCHWEIZ. MASCHINENMARKT; CHE; DA. 1981-02-18; VOL. 81; NO 7; PP. 36-37Article